The fracture conduct and fracture method from the diffusion-bonded joints have been elucidated by macro fracture and magnified area morphologies. The macro fracture morphologies (flat fracture) reveal the propagation of crack happened alongside the MEA/DD5 interface in tensile checks from the joints achieved at 1020, 1050, and 1080 °C (Figure 8a�